MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Silberline Aquavet® 190nl-136M
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary polymeric dispersant/inhibitor blend. The dispersant/inhibitor blend allow the pigment pellets to disperse directly in water or for faster dispersibility in a water/co-solvent blend. The inhibitor is effective at reducing the aluminum-water reaction in a broad range of waterborne ink resins at higher pH levels. Due to their unique carrier system, Aquavet® pigments can be used in ink systems where block resistance and water spotting resistance are required. High or excessive shear during processing will reduce the effectiveness of the inhibitor and should be avoided.

Applications: Printing Inks; Waterborne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc2.00 g/cc
Volatiles 3.0 %3.0 %
Particle Size 17 µm17 µmBefore Conversion
 
Descriptive Properties
% Carrier20
Aluminum Flake, wt%80
CategoryNon-leafing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ESIBER268 / 6023

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.