MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
3M Dyneon™ PFE 02CZ Perfluoroelastomer Curative Masterbatch  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Product Description: 3M™ Dyneon™ PFE 02CZ is a cure accelerator masterbatch used to adjust cure speeds in HT PFE products. The base polymer is classified as FFKM per ASTM D1418.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 760 PFE 02CZ
 762.5 PFE 02CZ
 775 PFE 02CZ
 771.25 PFE 02CZ
 770 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 771.25 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 782.5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 785 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 74
@Treatment Temp. 300 °C,
Time 252000 sec
2.5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
 75
@Treatment Temp. 300 °C,
Time 252000 sec
0 PFE 02CZ, Dry Heat Resistance of Vulcanizate
 76
@Treatment Temp. 300 °C,
Time 252000 sec
5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
 77
@Treatment Temp. 300 °C,
Time 252000 sec
1.25 PFE 02CZ, Dry Heat Resistance of Vulcanizate
Tensile Strength at Break 13.7 MPa0 PFE 02CZ; ASTM D573
 15.0 MPa1.25 PFE 02CZ; ASTM D573
 15.0 MPa2.5 PFE 02CZ; ASTM D573
 16.1 MPa5 PFE 02CZ; ASTM D573
 11.81 MPa
@Treatment Temp. 300 °C,
Time 252000 sec
0 PFE 02CZ, Dry Heat Resistance of Vulcanizate; ASTM D573
 12.855 MPa
@Treatment Temp. 300 °C,
Time 252000 sec
1.25 PFE 02CZ, Dry Heat Resistance of Vulcanizate; ASTM D573
 13.68 MPa
@Treatment Temp. 300 °C,
Time 252000 sec
2.5 PFE 02CZ, Dry Heat Resistance of Vulcanizate; ASTM D573
 14.844 MPa
@Treatment Temp. 300 °C,
Time 252000 sec
5 PFE 02CZ, Dry Heat Resistance of Vulcanizate; ASTM D573
Tensile Strength 15.9 MPa0 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 16.4 MPa2.5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 17.4 MPa1.25 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 17.9 MPa5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
Elongation at Break 166 %1.25 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 166 %0 PFE 02CZ
 167 %0 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 168 %5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 181 %2.5 PFE 02CZ
 195 %1.25 PFE 02CZ
 199 %5 PFE 02CZ
 753 %2.5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 165.336 %
@Treatment Temp. 300 °C,
Time 252000 sec
0 PFE 02CZ, Dry Heat Resistance of Vulcanizate
 214.5 %
@Treatment Temp. 300 °C,
Time 252000 sec
2.5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
 229.5 %
@Treatment Temp. 300 °C,
Time 252000 sec
1.25 PFE 02CZ, Dry Heat Resistance of Vulcanizate
 235.4 %
@Treatment Temp. 300 °C,
Time 252000 sec
5 PFE 02CZ, Dry Heat Resistance of Vulcanizate
100% Modulus 0.00850 GPa
@Strain 100 %
2.5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 0.00870 GPa
@Strain 100 %
0 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 0.00960 GPa
@Strain 100 %
5 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
 0.00970 GPa
@Strain 100 %
1.25 PFE 02CZ, Press Cure 15 Minutes @ 188°C (370°F) Post Cure 24 Hours @ 250°C (482°F)
Compression Set 19 %
@Temperature 230 °C,
Time 252000 sec
1.25 PFE 02CZ, -214 O-rings, 25% Deformation; ASTM D395 Method B
 20 %
@Temperature 230 °C,
Time 252000 sec
5 PFE 02CZ, -214 O-rings, 25% Deformation; ASTM D395 Method B
 21 %
@Temperature 230 °C,
Time 252000 sec
2.5 PFE 02CZ, -214 O-rings, 25% Deformation; ASTM D395 Method B
 28 %
@Temperature 230 °C,
Time 252000 sec
0 PFE 02CZ, -214 O-rings, 25% Deformation; ASTM D395 Method B
 
Descriptive Properties
AppearanceWhite
MH, Maximum Torque13.1 inch-lbASTM D5289, 5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 13.3 inch-lbASTM D5289, 2.5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 13.6 inch-lbASTM D5289, 0 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 15.3 inch-lbASTM D5289, 1.25 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
ML, Minimum Torque1.2 inch-lbASTM D5289, 0 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 1.2 inch-lbASTM D5289, 2.5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 1.2 inch-lbASTM D5289, 5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 1.3 inch-lbASTM D5289, 1.25 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
t`50, Time to 50% cure3.9 minutesASTM D5289, 5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 4.7 minutesASTM D5289, 2.5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 5.2 minutesASTM D5289, 1.25 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 6.3 minutesASTM D5289, 0 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
t`90 - Time to 90% cure10.1 minutesASTM D5289, 2.5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 11 minutesASTM D5289, 1.25 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 12.7 minutesASTM D5289, 0 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 8.4 minutesASTM D5289, 5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
ts2 - Time to 2 in-lb rise from min2.6 minutesASTM D5289, 5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 3.1 minutesASTM D5289, 2.5 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 3.3 minutesASTM D5289, 1.25 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)
 4.2 minutesASTM D5289, 0 PFE 02CZ, 100 cpm, 0.5° Arc, 20 Minutes @ 188°C (370°F)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ PFE 01CZ Perfluoroelastomer Curative Masterbatch
3M Dyneon™ PFE 191T High Temperature Perfluoroelastomer
ATG s.r.l. EACM Ethylene-Acrylic Rubber
3M Dyneon™ THV 340Z Fluoroplastic Dispersion
A. Schulman Alcryn® 2180 BK Melt Processable Rubber

PMM40017 / 194908

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.