MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AlphaGary Evoprene™ HP 3732 High Performance Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Evoprene™ HP is a hydrogenated styrene block copolymer based thermoplastic elastomer. Specially formulated for applications requiring high strength and excellent abrasion resistance, Evoprene™ HP can be used in some applications where thermoplastic polyurethane would normally be specified.
Evoprene™ HP has very good, heat ageing properties, excellent hydrolysis resistance and, when properly protected, very good antimicrobial resistance.
Can be used in food contact applications with the appropriate stabilizer package

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccISO 2782
Viscosity Measurement 15
@Temperature 150 °C
15
@Temperature 302 °F
Kg/cm2; Macklow-Smith extrusion rheometer
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ISO 868
Tensile Strength 22.0 MPa3190 psiISO 37
Elongation at Break 655 %655 %ISO 37
100% Modulus 5.30 MPa
@Strain 100 %
769 psi
@Strain 100 %
ISO 37
200% Modulus 6.00 MPa
@Strain 200 %
870 psi
@Strain 200 %
ISO 37
300% Modulus 7.30 MPa
@Strain 300 %
1060 psi
@Strain 300 %
ISO 37
Tear Strength 75.0 kN/m428 pliISO 34-B
Abrasion 8585mm3; DIN 53516
Compression Set  35 %
@Temperature 22.0 °C,
Time 259000 sec
35 %
@Temperature 71.6 °F,
Time 72.0 hour
ISO 815
 50 %
@Temperature 70.0 °C,
Time 79200 sec
50 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 65 %
@Temperature 100 °C,
Time 79200 sec
65 %
@Temperature 212 °F,
Time 22.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Descriptive Properties
Bonds withPolypropylene
Chemical ResistanceAcetoneModerate/Good
 Acids up to 80%Excellent
 AlcoholExcellent
 AlkalisExcellent
 Brake fluidGood
 Chlorinate solventsPoor
 DieselPoor
 Ethylene glycolExcellent
 GasolineGood
 Salt solutionExcellent
 Soda lyeExcellent
 Water, 23°CExcellent
 Water, 95°CGood

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary Evoprene™ HP 3704 High Performance Thermoplastic Elastomer
Mearthane Durethane™ S DS-270A Solid Polyurethane Elastomer
Mearthane Durethane™ S DS-285A Solid Polyurethane Elastomer
Mearthane Durethane™ S DS-280A Solid Polyurethane Elastomer
AlphaGary Evoprene™ HP 3702 High Performance Thermoplastic Elastomer

PGARY9654 / 140447

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.