Product Description: INNATE ST 30 Precision Packaging Resin is designed for excellent balance of stiffness and mechanical performance like tear resistance and dart impact resistance. Availability: North America Agency Ratings: EU No 10/2011; FDA 21 CFR 177.1520 ©3.2a Form: Pellets Information provided by The Dow Chemical Company |