MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow Unival™ DMDG-6240 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Product Description: Unival™ DMDG-6240 NT 7 HDPE is a multipurpose polymer designed for high speed production of blow molded containers used to package household industrial chemicals, such as laundry detergent, health and medicinal aids as well as agricultural and food products. The product is specifically designed to provide excellent processing in all extrusion blow molding equipment.
Main Characteristics:
  • Excellent processability
  • High melt strength
  • Excellent ESCR
Compiles with: US FDA 21 CFR 177.1520 ©3.2a; Canadian HPFB No Objection (with Limitations); EU No 10/2011

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520 ©3.2a; Canadian HPFB No Objection; EU No 10/2011

Form: Pellets

Processing Method: Blow Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 g/ccASTM D792
ESCR 100% Igepal® 400 hour
@Temperature 50.0 °C
F50; ASTM D1693
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 43 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM D2240
Tensile Strength at Break 2400 psiASTM D638
Tensile Strength, Yield 3450 psiASTM D638
Elongation at Break 770 %ASTM D638
Elongation at Yield 11 %ASTM D638
Flexural Modulus 118000 psi2% Secant; ASTM D790B
 148000 psi1% Secant; ASTM D790B
 167000 psiTangent; ASTM D790B
Tensile Impact Strength 72.0 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Melting Point 259 °F
Crystallization Temperature 226 °F
Deflection Temperature at 0.46 MPa (66 psi) 145 °FUnannealed; ASTM D648
Vicat Softening Point 250 °FASTM D1525
Brittleness Temperature <= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF578 / 311271

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.