MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Uniplex 280CG Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex 280CG is a stable, clear, odorless, and non-crystalline brittle solid with a sharp softening range starting at around 93°C. It has excellent ultraviolet light stability. Uniplex 280CG is compatible with a broad range of resins, plasticizers and solvents.

Chemical composition: Sucrose Benzoate

General Uniplex 280CG is a stable, clear, and non-crystalline brittle solid of characteristic low odor with an excellent ultraviolet light stability and hydrolytic resistance. Prolonged heating of Sucrose Benzoate at elevated temperatures causes darkening and increases in acidity. Uniplex 280CG shows a reasonably sharp softening range starting at around 93 °C. The viscosities of the molten product is about 900 mPas at 120°C and about 590 mPas at 150°C. Uniplex 280CG is specifically designed for the coating and ink industry. However, this product may also be used in numerous applications areas as indicated by the listing of compatibilities attached. Uniplex 280CG is compatible with a broad range of resins, plasticizers, and solvents and insoluble in water and aliphatic hydrocarbons. A partial listing of solvents and liquid plasticizers with which Uniplex 280CG is miscible at 25°C is acetone, butyl acetate, ethyl acetate, carbitol, ketones like di isobutyl ketone, and methyl ethyl ketone, toluene, xylene, polyethylene glycols, dipropylene and diethylene glycol dibenzoates, methyl benzoate, and tricresyl phosphate.

Applications: Uniplex 280CG is compatible with a large number of resins and polymers including acrylates, phenolic modified alkyd resins, melamine and urea formaldehyde resins, cellulosics like ethyl cellulose, nitrocellulose and cellulose acetobutyrate, polyesters, PVAc and PVAc modified PVC. Uniplex 280CG is an outstanding modifier for clear lacquers. It provides exceptional clarity with high gloss, excellent resistance to ultraviolet light, high film hardness combined with good flexibility, and excellent resistance to water and alcohol. In addition to usage in the formulation of clear coatings for wood, paper and metal, and in formulation of ink systems, the properties of Sucrose Benzoate indicate that it should be of interest in metallic and pigmented coatings, and heat seal coatings. Uniplex 280CG may be used to particular advantage in UV coating and inks. Uniplex 280CG improves the UV systems stability and allows easier processing. In addition, it imparts good film hardness, excellent gloss, and depth of gloss.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/cc
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 93.0 - 98.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.577
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear solid
Color<50Hazen, 50% w/v in Xylene
Content<1.5%Residual ortho-Xylene
Hydroxyl value<1.5 mg KOH/g
Specifications<0.01%Iodine Number
 <0.3%Acidity
 >85%Turbidity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, 30% Glass Fiber Reinforced
Overview of materials for Phenolic, Resole, Wood Filled
IRPC Polimaxx Polene 1102H Polypropylene Homopolymer
Geon® Performance Solutions 82520 Fiberloc PVC; 20% Glass Fiber Reinforced
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid

PLANY9106 / 209497

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.