MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Clwyd Compounders SBR Styrene Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: SBR has good physical strength, tear and abrasion resistance. Applications include non-mechanical high-volume products such as shoe soles and heels or car tires, gaskets, chewing gum.

Typical applications:

  • Non-mechanical high-volume products such as shoe soles and heels or car tires
  • Gaskets
  • Chewing gum
Advantages:
  • Good physical strength
  • Good tear and abrasion resistance
  • Good ageing stability
  • Better wet skid resistance to NR
Disadvantages:
  • Does not resist oil or fuels
  • Prone to weathering
  • Lower resilience to NR
  • Inferior heat build-up to NR

Information provided by CLWYD COMPOUNDERS LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40 - 9540 - 95
Tensile Strength <= 25.0 MPa<= 3630 psi
Elongation at Break <= 500 %<= 500 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °FUpper continuous
Minimum Service Temperature, Air -50.0 °C-58.0 °Fnon-brittle
 -25.0 °C-13.0 °Fsealing applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCLWYD028 / 316045

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.