MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Traid Villarroya TKG® 300 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:
  • Very low water absorption
  • Resistant to dilute acids, solvents and cleaning agents
  • UV resistant
  • Good electrical insulation
  • Easily weldable
Industry Applications:
  • Food processing industry
  • Chemical machines
  • Low load rollers

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/cc
Water Absorption 0.010 %
@Time 86400 sec
DIN EN ISO 62
 0.020 %
@Time 346000 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 50.0 MPaISO 2039-1
Tensile Strength, Yield 25.0 MPa50 mm/min; DIN EN ISO 527-2
Creep Strength 50.0 MPa
@Time 3.60e+6 sec
static load
Modulus of Elasticity 1.00 GPaIn tension; DIN EN ISO 527-2
Flexural Modulus 1.00 - 1.40 GPaDIN EN ISO 527-2
Charpy Impact Unnotched 140 kJ/m²Max. 7,5j; DIN EN ISO 179-1EU
Charpy Impact, Notched NBMax. 7,5j; DIN EN ISO 179-1EU
Coefficient of Friction 0.29Against steel p=0,05 N/mm2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmDIN IEC 60093
Surface Resistance >= 1.00e+13 ohmDIN IEC 60093
Dielectric Constant 2.4
@Frequency 100000 Hz
DIN 53483
Dielectric Strength >= 50.0 kV/mm
@Thickness 1.00 mm
ASTM 149
Dielectric Loss Index 0.00020
@Frequency 100000 Hz
DIN 53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 - 150 µm/m-°CDIN 53483
Specific Heat Capacity 1.70 - 2.00 J/g-°CISO 22007-4:2008
Thermal Conductivity 0.350 - 0.430 W/m-KISO 22007-4:2008
Melting Point 130 °CCrystalline; DIN 53765
Maximum Service Temperature, Air 80.0 °CLong term
 90.0 °CShort term
Heat Distortion Temperature 42.0 - 49.0 °CMethod A; R75
 70.0 - 85.0 °CMethod B; R75
Glass Transition Temp, Tg -95.0 °CDIN 53765
Flammability, UL94 HBDIN IEC 60995-11-10
 
Descriptive Properties
ColorWhite / black / red / yellow / brown / green
Resistance to hot mater / basesResistant
Resistance to weatheringResistant in color
Time yield limit for 1% elong3 MPaafter 1000 hours
Tracking resistanceKA 3cDIN 53480

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAID910 / 318871

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.