MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cabot ENDURE™ E45 Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: General Description: Many industrial rubber product applications operate under severe conditions that lead to significant wear and tear. Improved durability of the rubber components may provide a distinct total cost advantage. As part of Cabot’s ongoing commitment to deliver solutions that meet our customers’ needs, we have developed the ENDURE™ family of carbon blacks engineered for durability. Improving wear, chunking and tear resistance or reducing heat buildup can result in longer part life, reducing costly equipment downtime, increasing throughput and enhancing end user profitability. Cabot products can enhance rubber part life and durability by optimizing the balance between heat buildup and reinforcement and are identified by the letter “D” in the ENDURE nomenclature system. In certain applications such as conveyor belts, reduced hysteresis in the rubber compound may also be of interest as it can result in decreased power consumption, representing a significant energy and operating cost saving. In other applications such as rubber tracks and certain mill liners, a decrease in hysteresis can help with extending part life. Cabot products can help reduce energy costs and extend part life by optimizing the balance between hysteresis and reinforcement and are identified by the letter “E” in the ENDURE nomenclature system.

Performance Features: ENDURE™ E45 carbon black exhibits good stiffness and very low heat build up in rubber and is the product of choice for rubber applications requiring less hysteresis than that offered by standard N500 ASTM semi reinforcing carbon blacks.

Typical Applications:

  • Bottom cover of low rolling resistant conveyor belts

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6767
Tensile Strength at Break 17.3 MPa2510 psi
Elongation at Break 329 %329 %
100% Modulus 4.30 MPa624 psi
300% Modulus 16.0 MPa2320 psi
Tear Strength 32.0 kN/m183 pli
 
Descriptive Properties
DIN Abrader128 mm3
Loading71 phr
RR Factor0.0567
Tan d0.089

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT139 / 315874

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.