MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin BN9003G Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ BN0039 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This blow moldable grade exhibits a good balance of impact resistance and surface aesthetics. NORYL BN0039 resin, with its Low warpage and dimensional stability, is an excellent candidate for automotive exterior components including spoilers.

Features: Hydrolytic Stability,Low Creep Sensitivity,Low Warpage,Aesthetics & Visual effects

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Moisture Absorption 0.0500 %0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %0.25 %ISO 62-1
Viscosity 12 cP
@Load 5.00 kg,
Temperature 280 °C
12 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm0.0055 - 0.0075 in/inSABIC method
 0.0055 - 0.0075 cm/cm
@Thickness 3.20 mm
0.0055 - 0.0075 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
@Thickness 3.20 mm
0.0055 - 0.0075 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 280 °C
10 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.0 MPa6090 psi50 mm/min; ASTM D638
 42.0 MPa6090 psi50 mm/min; ISO 527
Tensile Strength, Yield 47.0 MPa6820 psi50 mm/min; ISO 527
 48.0 MPa6960 psi50 mm/min; ASTM D638
Elongation at Break 30.4 %30.4 %50 mm/min; ISO 527
 45 %45 %50 mm/min; ASTM D638
Elongation at Yield 3.4 %3.4 %50 mm/min; ISO 527
 3.6 %3.6 %50 mm/min; ASTM D638
Tensile Modulus 2.17 GPa315 ksi1 mm/min; ISO 527
 2.24 GPa325 ksi5 mm/min; ASTM D638
Flexural Strength 70.0 MPa10200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 75.0 MPa10900 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.15 GPa312 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.19 GPa318 ksi2 mm/min; ISO 178
Izod Impact Notched 320 J236 ft-lbASTM D256
 127 J
@Temperature -30.0 °C
93.7 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
Izod Impact, Notched (ISO) 25.0 kJ/m²11.9 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 54.0 kJ/m²
@Temperature -30.0 °C
25.7 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 10.7 J/cm²
@Temperature -30.0 °C
50.9 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 2.60 J/cm²12.4 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 40.0 J29.5 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  86.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 86.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 126 °C259 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 124 °C
@Thickness 3.20 mm
255 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 108 °C
@Thickness 3.20 mm
226 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 127 °C261 °FRate B/50; ISO 306
 130 °C266 °FRate B/120; ISO 306
 141 °C286 °FRate B/50; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 225 - 260 °C437 - 500 °FExtrusion Blow Molding
Zone 2 230 - 260 °C446 - 500 °FExtrusion Blow Molding
Zone 3 235 - 260 °C455 - 500 °FExtrusion Blow Molding
Zone 4 235 - 260 °C455 - 500 °FExtrusion Blow Molding
Zone 5 235 - 260 °C455 - 500 °F
Die Temperature 235 - 260 °C455 - 500 °FExtrusion Blow Molding
Melt Temperature 235 - 260 °C455 - 500 °FExtrusion Blow Molding
Head Temperature 235 - 260 °C455 - 500 °FZone 6 - Top Temperature
 235 - 260 °C455 - 500 °FZone 7 - Bottom Temperature
 235 - 260 °C455 - 500 °FZone 7 - Middle Temperature
Mold Temperature 65.0 - 95.0 °C149 - 203 °F
Drying Temperature 80.0 - 85.0 °C176 - 185 °FExtrusion Blow Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82259 / 290206

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.