Varcum 29116 is a one-step crushed phenolic resin based on bisphenol. APPLICATION: Varcum 29116 is used in metal coating formulations. FEATURES - Produces a light colored coating.
- Meets demanding critical taste considerations
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |