MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for exterior applications and painted or plated for special decorative effects.

Typical Applications:

  • Heat sealable coating
  • Base resin for color concentrates
  • Metal coating
  • Dispersions
  • Paper coating
  • Nonwoven binding

Features:

  • Good adhesion to metal, glass, cellulosic and other polar substrates
  • May be processed into aqueous amines and alkali based dispersions

Information provided by DuPont.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D792
Melt Index of Compound 395 g/10 min
@Load 2.16 kg,
Temperature 190 °C
395 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555Initial (peak) hardness; ASTM D2240
Tensile Strength at Break 10.5 MPa1520 psiType IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638
Elongation at Break 357 %357 %Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638
Flexural Modulus 0.0462 GPa6.70 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Tensile Impact Strength  9.50 kJ/m²
@Temperature -40.0 °C
4.52 ft-lb/in²
@Temperature -40.0 °F
ASTM D1822S
 209.3 kJ/m²
@Temperature 23.0 °C
99.59 ft-lb/in²
@Temperature 73.4 °F
ASTM D1822S
 
Thermal PropertiesMetricEnglishComments
Melting Point 55.0 - 83.0 °C131 - 181 °FASTM D3418(DSC)
Vicat Softening Point 48.0 °C118 °FRate B; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 160 °C320 °F
Zone 2 182 °C360 °F
Zone 3 193 °C379 °F
Zone 4 204 °C399 °F
Zone 5 204 °C399 °F
Die Temperature 204 °C400 °F
Melt Temperature 149 - 232 °C300 - 450 °F
 
Descriptive Properties
Methacrylic Acid Content19 wt.%DuPont Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Esstech X-721-0000 Polyethyleneglycol 400 Dimethacrylate, C26-28H46-50O12-13
Dow Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer
Dow Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer

PDUPM111 / 33778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.