MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Cabot E2C™ EX9620 Elastomer Composite
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: General Description: Cabot’s engineered elastomer composite (E2C™) solutions are designed for superior particle dispersion and enhanced polymer-particle interaction, which results in stronger reinforcement, improved resistance to damage and reduced hysteresis.

Performance Features: E2C EX9620 is designed to deliver superior heat buildup performance and rebound without sacrificing for durability in applications where abrasion is the primary wear mechanism.

Typical Applications:

  • Off-the-road tread/retread for high durability
  • Heavy urban (city bus, garbage truck)
  • Mining slurry applications with erosion: Slurry pump liner; Hydro-cyclone liner
  • Screen panel for minimizing plugging and blinding

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 69
@Temperature 100 °C
ML (1+4)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 29.8 MPa
Elongation at Break 528 %
300% Modulus 17.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT015 / 315750

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.