MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Synthos XPS PRIME S 70 Extruded polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Synthos XPS PRIME S is characterized by increased thermal insulation, protecting the internal temperature of buildings against the influence of external temperature variability. Constant mechanical strength, durability and resistance to biological agents and chemicals ensure that these boards fulfill their role for many years of use of the building.

Information provided by Synthos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.290 - 0.360 g/cc0.0105 - 0.0130 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 0.200 MPa>= 29.0 psiperpendicular to faces; EN 1607
Modulus of Elasticity 0.0125 GPa1.81 ksiat 50% of the peak stress; EN 826
 0.0300 GPa4.35 ksiin compression; EN 826
Flexural Strength >= 0.300 MPa>= 43.5 psidN = 100 mm; EN 12089
 >= 0.400 MPa>= 58.0 psidN = 60 mm; EN 12089
 >= 0.400 MPa>= 58.0 psidN = 80 mm; EN 12089
 >= 0.500 MPa>= 72.5 psidN = 50 mm; EN 12089
 >= 0.700 MPa>= 102 psidN = 40 mm; EN 12089
Compressive Strength >= 0.250 MPa>= 36.3 psiCompressive creep; EN 1606 + AC
 >= 0.300 MPa>= 43.5 psi2% deformation; EN 826
 >= 0.600 MPa>= 87.0 psi5% deformation; EN 826
 >= 0.700 MPa>= 102 psi10% relative deformation; EN 826
 >= 0.750 MPa>= 109 psiAverage achieved, at 10% deformation; EN 826
Poissons Ratio 0.410.41PN-EN 12090, PN-EN 826
Shear Strength >= 0.200 MPa>= 29.0 psidN = 100 mm; EN 12090
 >= 0.220 MPa>= 31.9 psidN = 80 mm; EN 12090
 >= 0.260 MPa>= 37.7 psidN = 60 mm; EN 12090
 >= 0.310 MPa>= 45.0 psidN = 50 mm; EN 12090
 >= 0.390 MPa>= 56.6 psidN = 40 mm; EN 12090
 
Thermal PropertiesMetricEnglishComments
CTE, linear <= 50.0 µm/m-°C<= 27.8 µin/in-°Fvia thickness; EN 14581
CTE, linear, Parallel to Flow <= 80.0 µm/m-°C<= 44.4 µin/in-°FEN 14581
CTE, linear, Transverse to Flow <= 60.0 µm/m-°C<= 33.3 µin/in-°FEN 14581
Thermal Conductivity  0.0260 W/m-K
@Temperature -60.0 °C
0.180 BTU-in/hr-ft²-°F
@Temperature -76.0 °F
dN = 40 mm; EN 14307
 0.0270 W/m-K
@Temperature -60.0 °C
0.187 BTU-in/hr-ft²-°F
@Temperature -76.0 °F
dN = 50-100 mm; EN 14307
 0.0270 W/m-K
@Temperature -40.0 °C
0.187 BTU-in/hr-ft²-°F
@Temperature -40.0 °F
dN = 40 mm; EN 14307
 0.0290 W/m-K
@Temperature -40.0 °C
0.201 BTU-in/hr-ft²-°F
@Temperature -40.0 °F
dN = 50-100 mm; EN 14307
 0.0290 W/m-K
@Temperature -20.0 °C
0.201 BTU-in/hr-ft²-°F
@Temperature -4.00 °F
dN = 40 mm; EN 14307
 0.0310 W/m-K
@Temperature -20.0 °C
0.215 BTU-in/hr-ft²-°F
@Temperature -4.00 °F
dN = 50-100 mm; EN 14307
 0.0310 W/m-K
@Temperature 0.000 °C
0.215 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
dN = 40 mm; EN 14307
 0.0330 W/m-K
@Temperature 0.000 °C
0.229 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
dN = 50-100 mm; EN 14307
 0.0330 W/m-K
@Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
dN = 40 mm; EN 14307
 0.0340 W/m-K
@Temperature 10.0 °C
0.236 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
dN = 50-100 mm; EN 14307
 0.0340 W/m-K
@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
dN = 40 mm; EN 14307
 0.0350 W/m-K
@Temperature 20.0 °C
0.243 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
dN = 50-80 mm; EN 14307
 0.0360 W/m-K
@Temperature 40.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 104 °F
dN = 40 mm; EN 14307
 0.0370 W/m-K
@Temperature 40.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 104 °F
dN = 50-80 mm; EN 14307
 0.0370 W/m-K
@Temperature 20.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
dN = 100 mm; EN 14307
 0.0380 W/m-K
@Temperature 60.0 °C
0.264 BTU-in/hr-ft²-°F
@Temperature 140 °F
dN = 40 mm; EN 14307
 0.0390 W/m-K
@Temperature 60.0 °C
0.271 BTU-in/hr-ft²-°F
@Temperature 140 °F
dN = 50-80 mm; EN 14307
 0.0390 W/m-K
@Temperature 40.0 °C
0.271 BTU-in/hr-ft²-°F
@Temperature 104 °F
dN = 100 mm; EN 14307
 0.0400 W/m-K
@Temperature 70.0 °C
0.278 BTU-in/hr-ft²-°F
@Temperature 158 °F
dN = 40-80 mm; EN 14307
 0.0420 W/m-K
@Temperature 60.0 °C
0.291 BTU-in/hr-ft²-°F
@Temperature 140 °F
dN = 100 mm; EN 14307
 0.0450 W/m-K
@Temperature 70.0 °C
0.312 BTU-in/hr-ft²-°F
@Temperature 158 °F
dN = 100 mm; EN 14307
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flash Point >= 400 °C>= 752 °FCSN 640149
 
Descriptive Properties
Content<27 mg/kgwater soluble chlorides, EN 13468
 <27 mg/kgwater soluble silicates, EN 13468
 <5 mg/kgwater soluble fluorides, EN 13468
 <5 mg/kgwater soluble sodium ions, EN 13468
Dynamic stiffness190 MN/m3dN = 100 mm; EN 29052-1
 230 MN/m3dN = 80 mm; EN 29052-1
 320 MN/m3dN = 60 mm; EN 29052-1
 380 MN/m3dN = 50 mm; EN 29052-1
 440 MN/m3dN = 40 mm; EN 29052-1
Point load level>5000 NEN 12430, for 5 mm deformation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSYNTHOS088 / 320369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.