MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Nymax™ 1010 A Black 13 Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.

Molded Test Bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Water Absorption 1.0 %
@Thickness 3.18 mm
1.0 %
@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.3 MPa7300 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 70 %70 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 68.9 MPa9990 psiASTM D790
Flexural Modulus 1.93 GPa280 ksiASTM D790
Izod Impact, Notched 9.10 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
17.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 216 °C421 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
@Thickness 3.18 mm
131 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Descriptive Properties
AdditiveImpact Modifier
AppearanceBlack
FeaturesGeneral Purpose
 Impact Modified
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Nymax™ ND 1233 GF Black Polyamide 66 (Nylon 66)
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
Celanese Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Ineos H35G-00 Polypropylene Homopolymer
Techmer ES Elastoblend® PA6 IM L N

PH0POL0665 / 145234

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.