MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound AF004 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: LNP THERMOCOMP AF004 compound is based on Acrylonitrile Butadiene Styrene (ABS) resin containing 20% glass fiber.

Features: High Stiffness,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption 0.0500 - 0.100 %0.0500 - 0.100 %Injection Molding
 0.240 %0.240 %23°C/50% RH/24 hrs; ASTM D570
 0.390 %0.390 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in24hrs; ASTM D955
 0.0024 cm/cm0.0024 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/in24hrs; ASTM D955
 0.0040 cm/cm0.0040 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 76.0 MPa11000 psiISO 527
 78.0 MPa11300 psiASTM D638
Elongation at Break 2.0 %2.0 %ISO 527
 2.2 %2.2 %ASTM D638
Tensile Modulus 6.00 GPa870 ksi1 mm/min; ISO 527
 6.17 GPa895 ksi5 mm/min; ASTM D638
Flexural Strength 108 MPa15700 psiISO 178
 130 MPa18900 psiASTM D790
Flexural Modulus 5.33 GPa773 ksiISO 178
 6.15 GPa892 ksiASTM D790
Izod Impact Notched 80.0 J59.0 ft-lbASTM D256
Izod Impact, Unnotched 3.95 J/cm7.40 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 19.0 kJ/m²9.04 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 11.0 J8.11 ft-lbpeak; ASTM D3763
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 103 °C
@Thickness 3.20 mm
217 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 230 - 245 °C446 - 473 °F
Zone 3 265 - 275 °C509 - 527 °F
Melt Temperature 260 °C500 °FInjection Molding
Mold Temperature 70.0 - 80.0 °C158 - 176 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81460 / 289407

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.