MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotchkote™ RS 820 Epoxy Screed
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Sceed RS 820 has been specially developed as a three component 100% solids resurfacing screed for application to concrete floor surfaces

Product Features:

  • Combines good application characteristics with excellent chemical resistance
  • Designed for application by trowel for float
  • Can be used to form wall/floor covings and can be laid to fails.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Thickness 240 mil
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 80ASTM D2240
Tensile Strength at Break 22.6 MPaASTM D638
Elongation at Break 15 - 20 %ASTM D412
Compressive Strength 12500 psiASTM D695
Impact Test 1.40 JASTM D2794
Abrasion 78[mg] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 hourHard Dry
 168 hourFull Cure
 
Descriptive Properties
AppearanceLight Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik SITREN® AirVoid® 351 Surfactant
Anhydrite (CaSO4)

PMM35313 / 170060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.