MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® L4903 High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes:

Applications
ALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resin as well as low gel levels. Typical applications include trash liners and products requiring incorporating PCR.

Regulatory Status
L 4903 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing L 4903 can only be made when the processing conditions, equipment and end use are known.

Typical Extrusion Conditions: BUR=4.1, Neck Height=8 Die Diameters, 0.5 Mil Film, Melt Temperature- 390-410°F(199-210°C)

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D1505
Thickness 0.500 mil4:1 BUR; Neck Height = 8 Die Diameters
Melt Flow 0.027 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 5940 psiASTM D882
Film Tensile Strength at Yield, TD 4860 psiASTM D882
Film Elongation at Break, MD 390 %ASTM D882
Film Elongation at Break, TD 260 %ASTM D882
Dart Drop, Total Energy 1.80 ft-lbASTM D3420
Elmendorf Tear Strength MD 20 gASTM D1922
Elmendorf Tear Strength TD 18 gASTM D1922
Film Tensile Strength at Break, MD 9440 psiASTM D882
Film Tensile Strength at Break, TD 9680 psiASTM D882
1% Secant Modulus, MD 167000 psiASTM D822
1% Secant Modulus, TD 142000 psiASTM D822
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 210 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 350F High Density Polyethylene, Film Extrusion Grade
Total HP 401 MDPE, pipe, cable, sheet
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Celanese GUR® 4120 PE-UHMW, Unfilled
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene

PEQU0133 / 36562

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.