MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for PVC, Molded
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.480 - 2.50 g/ccAverage value: 1.29 g/cc Grade Count:629
Volatile Organic Compounds (VOC) Content 0.300 g/lAverage value: 0.300 g/l Grade Count:9
Water Absorption 0.0200 - 0.400 %Average value: 0.278 % Grade Count:12
Particle Size 63.0 - 250 µmAverage value: 157 µm Grade Count:12
Viscosity 0.680 - 2.27 cPAverage value: 1.48 cP Grade Count:11
Viscosity Test 101 - 145 cm³/gAverage value: 119 cm³/g Grade Count:10
Viscosity Number 79.0 - 180 cm³/gAverage value: 121 cm³/g Grade Count:14
Thickness 1000 - 3000 micronsAverage value: 1100 microns Grade Count:26
Linear Mold Shrinkage 0.00200 - 0.0500 cm/cmAverage value: 0.00579 cm/cm Grade Count:29
Melt Flow 2.00 - 25.0 g/10 minAverage value: 12.5 g/10 min Grade Count:7
Spiral Flow 63.5 - 94.0 cmAverage value: 83.0 cm Grade Count:6
ASTM Color -32.4 - 97.2Average value: 18.7 Grade Count:56
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 28.0 - 99.0Average value: 71.0 Grade Count:506
Hardness, Shore D 34.0 - 87.0Average value: 68.0 Grade Count:71
Hardness, Shore C 75.0 - 95.0Average value: 85.0 Grade Count:5
Tensile Strength, Ultimate 1.47 - 59.0 MPaAverage value: 16.6 MPa Grade Count:594
Tensile Strength, Yield 29.6 - 52.0 MPaAverage value: 43.2 MPa Grade Count:23
Elongation at Break 3.00 - 600 %Average value: 312 % Grade Count:566
Modulus of Elasticity 0.00163 - 3.24 GPaAverage value: 2.14 GPa Grade Count:50
Flexural Yield Strength 2.83 - 103 MPaAverage value: 74.8 MPa Grade Count:42
Flexural Modulus 1.65 - 3.31 GPaAverage value: 2.67 GPa Grade Count:39
Izod Impact, Notched 0.300 - 28.4 J/cmAverage value: 6.36 J/cm Grade Count:42
 0.534 - 7.47 J/cm
@Temperature -40.0 - 0.000 °C
Average value: 3.11 J/cm Grade Count:4
 0.534 - 7.47 J/cm
@Thickness 3.18 - 3.18 mm
Average value: 3.11 J/cm Grade Count:4
Izod Impact, Unnotched 0.400 - 11.3 J/cmAverage value: 4.42 J/cm Grade Count:16
Tensile Impact Strength 63.0 - 168 kJ/m²Average value: 139 kJ/m² Grade Count:7
Tear Strength Test 145 - 530Average value: 308 Grade Count:64
Tear Strength 15.0 - 75.0 kN/mAverage value: 33.6 kN/m Grade Count:23
Dart Drop Total Energy 534 - 2140 J/cmAverage value: 1660 J/cm Grade Count:7
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.00e+6 - 1.00e+15 ohm-cmAverage value: 1.04e+14 ohm-cm Grade Count:19
 >= 2.00e+10 ohm-cm
@Temperature 70.0 - 70.0 °C
Average value: 1.05e+12 ohm-cm Grade Count:5
Comparative Tracking Index 400 - 600 VAverage value: 575 V Grade Count:4
Hot Wire Ignition, HWI 60.0 - 120 secAverage value: 93.3 sec Grade Count:8
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 40.0 - 100 °CAverage value: 52.2 °C Grade Count:29
Deflection Temperature at 0.46 MPa (66 psi) 66.0 - 90.6 °CAverage value: 77.3 °C Grade Count:18
Deflection Temperature at 1.8 MPa (264 psi) 62.0 - 87.2 °CAverage value: 71.2 °C Grade Count:48
Vicat Softening Point 68.0 - 91.0 °CAverage value: 77.3 °C Grade Count:27
Softening Point 160 - 190 °CAverage value: 174 °C Grade Count:7
Minimum Service Temperature, Air -57.5 - -10.0 °CAverage value: -34.0 °C Grade Count:19
Brittleness Temperature -72.0 - -3.00 °CAverage value: -36.4 °C Grade Count:187
Decomposition Temperature 185 - 200 °CAverage value: 188 °C Grade Count:5
UL RTI, Electrical 50.0 - 80.0 °CAverage value: 56.0 °C Grade Count:5
UL RTI, Mechanical with Impact 50.0 - 70.0 °CAverage value: 54.0 °C Grade Count:5
UL RTI, Mechanical without Impact 50.0 - 80.0 °CAverage value: 56.0 °C Grade Count:5
Flammability, UL94 HB - 5VAGrade Count:57
Oxygen Index 25.0 - 34.0 %Average value: 28.4 % Grade Count:27
 
Optical PropertiesOriginal ValueComments
Haze 5.00 - 9.00 %Average value: 6.86 % Grade Count:7
Transmission, Visible 66.0 - 90.0 %Average value: 86.1 % Grade Count:56
 
Processing PropertiesOriginal ValueComments
Melt Temperature 154 - 213 °CAverage value: 179 °C Grade Count:119
 
Component Elements PropertiesOriginal ValueComments
Bromine, Br 0.0100 %Average value: 0.0100 % Grade Count:9
Cadmium, Cd 0.00500 %Average value: 0.00500 % Grade Count:9
Chromium, Cr 0.0100 %Average value: 0.0100 % Grade Count:9
Lead, Pb 0.0100 %Average value: 0.0100 % Grade Count:9
Mercury, Hg 0.0100 %Average value: 0.0100 % Grade Count:9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Overview of materials for PVC, Extruded
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for PVC, High Impact

O5600 / 78511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.