MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-50158 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-50100 Series of medical-grade TPEs can be used as an alternative to flexible PVC and silicone in face masks used in respiratory therapy. Medalist MD-50158 is a medium hardness, low density, RoHS compliant grade that can be sterilized and is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Sterilizability; Good Toughness; Halogen Free; High Flow; Low Density; Low Specific Gravity; Medium Hardness; No Animal Derived Components; Radiation (Gamma) Resistant; Resilient; Slip; Without Fillers

Uses: Disposable Hospital Goods; Handles; Knobs; Medical Devices; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.885 g/ccASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 58
@Time 5.00 sec
Injection Molded; ASTM D2240
 60
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 1100 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain 260 psi
@Strain 50 %
Die C, 20 in/min; ASTM D412
 305 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 500 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 660 %Die C, 20 in/min; ASTM D412
Tear Strength 220 pliFlow, Die C, 20 in/min; ASTM D624
Compression Set 26 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 320 - 350 °F
Middle Barrel Temperature 360 - 400 °F
Front Barrel Temperature 380 - 420 °F
Nozzle Temperature 360 - 440 °F
Melt Temperature 360 - 440 °F
Mold Temperature 80.0 - 120 °F
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 0.500 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Colorite Polymers 2002 Rigid PVC
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420
Teknor Apex Medalist® MD-12160H Thermoplastic Elastomer
Teknor Apex Medalist® MD-12362 Thermoplastic Elastomer
Teknor Apex Medalist® MD-17270 Thermoplastic Elastomer

PTEKNQ0730 / 237221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.