MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives 320 / 322 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides excellent adhesion to prepared metals, rubber, fiberglass reinforced plastics (FRP), polyester thermosets and thermoplastics, and many other materials. LORD 320/322 adhesive can be either room temperature cured or heat cured for faster processing.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 - 1.26 g/cc0.0444 - 0.0455 lb/in³322 Hardener
 1.50 - 1.55 g/cc0.0542 - 0.0560 lb/in³320 Resin
Solids Content 100 %100 %
Brookfield Viscosity  300000 - 1.00e+6 cP
@Temperature 25.0 °C
300000 - 1.00e+6 cP
@Temperature 77.0 °F
320 Resin; HBF, Helipath @ 5rpm, T-Bar Spindle D
 450000 - 2.00e+6 cP
@Temperature 25.0 °C
450000 - 2.00e+6 cP
@Temperature 77.0 °F
322 Hardener; HBF, Helipath @ 5rpm, T-Bar Spindle E
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.6 MPa4440 psiASTM D882-83A (mod)
Elongation at Break 3.0 %3.0 %ASTM D882-83A (mod)
Modulus of Elasticity 1.59 GPa230 ksiASTM D882-83A (mod)
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 80.0 °C176 °FASTM E1640-99 (by DMA)
Flash Point >= 93.0 °C>= 199 °F320 Resin; Closed Cup
 >= 93.0 °C>= 199 °F322 Hardener; Closed Cup
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature >=18.0 °C
24.0 hour
@Temperature >=64.4 °F
Pot Life 20 - 40 min
@Temperature 24.0 °C
20 - 40 min
@Temperature 75.2 °F
54g mass
Shelf Life  12.0 Month
@Temperature 21.0 - 27.0 °C
12.0 Month
@Temperature 69.8 - 80.6 °F
 12.0 Month
@Temperature 21.0 - 27.0 °C
12.0 Month
@Temperature 69.8 - 80.6 °F
 
Descriptive Properties
AppearanceGray322 Hardener
 GrayMixed
 Off-white320 Resin
ConsistencyPaste320 Resin
 Paste322 Hardener
 PasteMixed
Mix Ratio1.2:1by weight; general purpose (-40 to 400ºF)
 1:1by volume; general purpose (-40 to 400ºF)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay BR® 4535A Paste Adhesive
Lord Adhesives 406 Flexible, High Impact and Peel Resistance, Medium Working Time Acrylic Adhesive
Lord Adhesives 320/310-B Epoxy Adhesive System
Lord Adhesives 310 High Strength SMC, FRP and General Purpose Epoxy Adhesive
Henkel Hysol EA 9360 Paste Adhesive System

PLORD110 / 86118

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.