MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Noble Polymers Regis™ 115090 Thermoplastic Olefin (TPO)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE; Thermoplastic Olefinic Elastomer (TPO); TPO

Material Notes: Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, material handling, step pads and other applications requiring rigid TPOs. This recyclable product is a tough, high-strength thermoplastic that maintains its properties over a wide temperature range.

Information provided by Noble Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
Linear Mold Shrinkage 0.0083 cm/cmASTM D955
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2579 psiASTM D638
Elongation at Break 665.8 %ASTM D412
Izod Impact, Notched 1.91 ft-lb/in
@Temperature -30.0 °C
ASTM D256
 2.87 ft-lb/in
@Temperature 23.0 °C
ASTM D256
Gardner Impact 140.4 in-lb
@Temperature -30.0 °C
ASTM D5420
 140.4 in-lb
@Temperature 23.0 °C
ASTM D5420
Tangent Modulus 116000 psiASTM D790
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 375 - 425 °F
Ejection Temperature 80.0 - 130 °FWater Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® EHM 6004 High Density Polyethylene, Blow Molding
6004 Aluminum Composition Spec
Barlog Plastics KEBAFLEX S 45 A.01 TPE-S, Shore A45, translucent
Covestro Bayfill® EA 6004 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO)

PNOBLE14 / 54824

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.