MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel ASTM A 1018, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS)
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes:

Information provided by AK Steel

Key Words: ASTM A568, A1011, A635, A1018, A659, A749, SAE J1392, SAE J2340
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/cc
@Temperature 20.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 340 MPa
Tensile Strength, Yield >= 205 MPa
Elongation at Break >= 22 %
Modulus of Elasticity 200 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000142 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.4 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.481 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 89.0 W/m-K
@Temperature 20.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
AK Steel ASTM A 1018, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS)
AISI 1018 Steel, hot rolled, quenched, and tempered
AK Steel ASTM A 1018, Grade 36 Type 1 and 2 Hot Rolled Carbon Steel, Structural Steel (SS)
AK Steel ASTM A 1018, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS)

NAKS208 / 138527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.