(Viewing data as-entered.
Click here
to return)
Ascend Performance Materials Vydyne® PF003JX5 Nylon PA6-I-GF15
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Glass Filled, Impact Grade
Material Notes:
Vydyne PF003JX5 is an impact modified, 15% glass fiber reinforced, PA6 for injection molded applications.
Information provided by Ascend Performance Materials.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.17
g/cc
DAM; ISO 1183
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
78.0
MPa
DAM; ISO 527-2
Elongation at Break
6.8 %
DAM; ISO 527-2
Flexural Strength
90.0
MPa
DAM; ISO 178
Flexural Modulus
3000
MPa
DAM; ISO 178
Izod Impact, Notched (ISO)
12.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
21.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO)
61.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1U
62.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
105
°C
Unannealed; DAM; ISO 75-2/A
Processing Properties
Original Value
Comments
Rear Barrel Temperature
240
-
250
°C
Injection
Middle Barrel Temperature
240
-
260
°C
Injection
Front Barrel Temperature
240
-
260
°C
Injection
Nozzle Temperature
240
-
260
°C
Injection
Melt Temperature
240
-
260
°C
Injection
Mold Temperature
60.0
-
80.0
°C
Injection
Drying Temperature
80.0
°C
Injection
Dry Time
4.00
hour
Injection
Descriptive Properties
Agency Ratings
ISO, 1043 PA6 I GF15
Features
Impact Modified
Forms
Pellets
Processing Method
Injection Molding
Region
North America, Europe
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PASCE8831 / 293400
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.