MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain Chemlam® 10 Value Industrial Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass reinforcements. Chemfab® laminates outperform traditional PTFE_coated products of similar weight and thickness.
FEATURES:
PTFE cast barrier film surface, crack and pinhole free:
Outperforms simple PTFE-coated materials; long-lasting release properties make cleaning easier; low wicking properties extend useful life.
Uniform film thickness over entire surface: Lamination eliminates the possibility of thin spots found in coated materials, which often lead to their premature failure.
High temperature fabrics: Designed for thermal cycling and harsh chemical applications, including cooking and plastic processing.
FDA Compliant: Suitable for use in direct food contact applications under the applicable requirements of 21CFR177.1550. All data based on a 0.0095 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.883 g/ccWoven Density
 
Mechanical PropertiesOriginal ValueComments
Tear Strength Test 12Lbs./In. Propagation Tear Strength in fill/transverse direction
 18Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 215 pliFill/Transverse direction
 315 pliWarp/Longitudinal direction
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorBrown/Brown
Weight (oz/yd^2)13.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
Saint-Gobain CHR® 2255-2 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain Chemlam® 3300 High Mechanical Performance Industrial Laminate
Norplex-Micarta RT500 Epoxy Fiber Glass Laminate Tube, NEMA G-10
Cossa Polimeri ESTABLEND PSA 8500 V0 HF Flame Retardant PC / ASA Blend

PSTGQZ219 / 68733

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.