MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum A206.0-T7 Casting Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 206.0-T7; AA206.0-T7AMS 4235, AMS 4236, AMS 4237; UNS A02060; AlA206.0-T7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 120Estimated from Vickers Hardness.
Hardness, Knoop 151Estimated from Vickers Hardness.
Hardness, Rockwell A 47Estimated from Vickers Hardness.
Hardness, Rockwell B 75Estimated from Vickers Hardness.
Hardness, Vickers 137
Tensile Strength, Ultimate 436 MPa
Tensile Strength, Yield 350 MPa
@Strain 0.2 %
Elongation at Break 11.7 %in 50 mm
Reduction of Area 26 %
Tensile Modulus 70.0 GPaCompressive modulus in is typically about 2% higher for Al alloys
Compressive Yield Strength 372 MPa
Ultimate Bearing Strength 960 MPae/D = 2.0
Bearing Yield Strength 660 MPae/D = 2.0
Poissons Ratio 0.33
Fatigue Strength 90.0 MPa
@# of Cycles 1.00e+7
Axial; Kt=3.0; R=0.1
 205 MPa
@# of Cycles 1.00e+7
Axial; R=0.1
 370 MPa
@# of Cycles 1000
Axial; Kt=3.0; R=0.1
 435 MPa
@# of Cycles 1000
Axial; R=0.1
Fracture Toughness 43.0 MPa-m½
Shear Modulus 26.3 GPaCalculated
Shear Strength 257 MPa
Charpy Impact 9.50 JV-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000520 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/gTypical for cast aluminum
CTE, linear 19.3 µm/m-°C
@Temperature 20.0 - 100 °C
 24.7 µm/m-°C
@Temperature 20.0 - 300 °C
Value for Aluminum 201.0
Specific Heat Capacity 0.920 J/g-°C
Thermal Conductivity 121 W/m-K
Melting Point 570 - 650 °C
Solidus 570 °C
Liquidus 650 °C
 
Processing PropertiesOriginal ValueComments
Solution Temperature 950 - 960 °Ffor 2 hr followed by 980-990°F for 14-20 hr and a water quench
Aging Temperature 390 °Fhold at temperature for 8 hr
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 93.3 - 95.3 %As remainder
Copper, Cu 4.2 - 5.0 %
Iron, Fe <= 0.10 %
Magnesium, Mg 0.15 - 0.35 %
Manganese, Mn 0.20 - 0.50 %
Nickel, Ni <= 0.050 %
Other, each <= 0.050 %
Other, total <= 0.15 %
Silicon, Si <= 0.050 %
Tin, Sn <= 0.050 %
Titanium, Ti 0.15 - 0.30 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 201.0-T7, Sand Cast
Aluminum 201.0-T6 Casting Alloy
Aluminum 206.0-T7 Casting Alloy
Aluminum 204.0-T6, Permanent Mold Cast, Precipitation Treatment 12 h at 180°C (360°F)
Aluminum 355.0-T61, Cast

MAC2060AT7 / 9772

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.