MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Saint-Gobain Norton® Fluorglas® Chemfilm® DF2919 Fluoropolymer Tape
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess superior dielectric properties. The multi-layer process is ideal for bulk and surface properties suited to most demanding applications.

DF2000 Series: Combines fluoropolymers with the highest temperature rating and the best electrical properties with the mechanical integrity and dielectric strength of polyimide film. Heat sealable surfaces allow these tapes to be sealed to itself and other layers of fluoropolymer tape wrap insulation at regular wire processing temperatures and the fully sintered fluoropolymer base resin enables the films to be wrapped directly over the conductor.

DF2919/DF2929 Performance: Test programs in both military and commercial aircraft markets indicate the benefits of a proper ratio between fluoropolymers and polyimides to give maximum protection against arc propagation and failure.

Applications include: Wire and Cable Industry Applications
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D-792
Water Absorption <= 0.25 %<= 0.25 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 124 MPa18000 psiASTM D-882
Elongation at Break 100 %100 %ASTM D-882
Tensile Modulus 1.72 GPa250 ksiASTM D-882
Tear Strength 382 kN/m2180 pliInitial Tear Strength; ASTM D-1004
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 4.50e+17 ohm4.50e+17 ohmASTM D-257
Dielectric Constant 2.6
@Frequency 60.0 - 1.00e+8 Hz
2.6
@Frequency 60.0 - 1.00e+8 Hz
ASTM D-150
Dielectric Strength 236 kV/mm6000 kV/inASTM D-149
Dissipation Factor 0.0100.010ASTM D-150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °FUL-746 B
Minimum Service Temperature, Air -240 °C-400 °F
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Norton® PFA Fluoropolymer Film

PSTGQZ150 / 68664

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.