Product highlights: CABELEC XS6325A conductive concentrate is an electrically conductive concentrate made from a carefully selected carbon black finely dispersed in polyamide carrier. Its electrical properties are not dependent on atmospheric conditions; however, they depend on the type and level of dilution of the resin used and the processing conditions. Unlike standard conductive compounds, which have very limited dilution potential, CABELEC XS6325A conductive concentrate has the potential to be diluted with a high quantity of natural resin. This allows users of CABELEC XS6325A conductive concentrate to benefit from the versatility of this product and from the enhanced physical properties due to higher levels of dilution resin. Key applications: CABELEC XS6325A conductive concentrate is suitable for use in Polyamide 6 and Polyamide 6.6 compounding applications. Information provided by Cabot Corporation |