MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at low temperatures, increased hydrostatic strength and improved chemical resistance.

BE60-7032 is recommended for pressure pipes and fittings, chemical engineering components, extruded and compression molded sheets, filter plates and solid rods. The material is colored grey based on RAL 7032.

Former trade name for this product was Beta(ß)-PP.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 0.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4351.1 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 10 %At 50 mm/min; ISO 527-2
Modulus of Elasticity 1.30 GPaISO 527
Charpy Impact, Notched 5.00 J/cm²ISO 179/1eA
 0.500 J/cm²
@Temperature -20.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °CHDT; ISO 75 B
Vicat Softening Point 91.0 °CB (50 N); ISO 306
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 190 - 230 °C
Die Temperature 392 - 446 °F
Melt Temperature 200 - 230 °C
Head Temperature 200 - 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ti30Ta ß titanium alloy
Ti12Mo5Zr5Sn ß titanium alloy
Ti15Mo5Zr3Al ß titanium alloy
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications
Ti30Nb ß titanium alloy

PBOREA008 / 27315

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.