MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Mobility and Materials TPSiV® 3345-65A Silicone Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Silicone thermoplastic elastomer with good chemical resistance and excellent abrasion resistance.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Spiral Flow 28.0 cm11.0 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 7.30 MPa1060 psiCross direction; ISO 527-1/-2 or ISO 37
Tensile Stress at Strain 3.30 MPa
@Strain 100 %
479 psi
@Strain 100 %
Cross direction; ISO 527-1/-2 or ISO 37
Elongation at Break >= 300 %>= 300 %Cross direction; ISO 527-1/-2 or ISO 37
Tear Strength 41.0 kN/m234 plinormal; ISO 34-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 205 °C383 - 401 °FRange, Extrusion
 205 °C401 °FOptimum, Injection
Mold Temperature 25.0 °C77.0 °FOptimum, Injection
 10.0 - 40.0 °C50.0 - 104 °FInjection
Drying Temperature 90.0 °C194 °FInjection
 90.0 °C194 °FExtrusion
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hourExtrusion, Dehumidified Dryer
 3.00 - 6.00 hour3.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.030 %<= 0.030 %Extrusion
 <= 0.030 %<= 0.030 %Injection
Back Pressure 0.700 - 1.40 MPa102 - 203 psiInjection
Vent Depth 0.00130 - 0.00250 cm0.000512 - 0.000984 inInjection
 
Descriptive Properties
CompatibilityAcrylic Polymers
 Polycarbonate
 Styrenics
Drying RecommendedyesInjection
Max. screw tangential speed (m/s)0.4Injection
PolymerTPV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4900 / 249179

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.