MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those in contact with non-fatty, non-oily foods as closures and sealing gaskets. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

Recommended for applications requiring excellent flex fatigue resistance.

Information provided by Advanced Elastomer Systems

Key Words: EU 2003/11/EC; FDA 21 CFR 177.1210; FDA 21 CFR 177.2600; NSF 51; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555.12 in; ASTM D2240
 5858Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 4.94 MPa716 psiAir at 302°F, 168 hr; ASTM D573
 5.31 MPa770 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 1.93 MPa280 psiAcross Flow; ASTM D412
Elongation at Break 400 %400 %Across Flow; ASTM D412
 452 %452 %Air at 302°F, 168 hr; ASTM D573
Tear Strength 16.0 kN/m91.0 pli73°F, Die C; ASTM D624
Compression Set  22 %
@Temperature 70.0 °C,
Time 79200 sec
22 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 38 %
@Temperature 125 °C,
Time 252000 sec
38 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Rear Barrel Temperature 177 °C350 °F
Middle Barrel Temperature 182 °C360 °F
Front Barrel Temperature 182 °C360 °F
Nozzle Temperature 188 - 221 °C370 - 430 °F
Die Temperature 199 °C390 °FExtrusion
Melt Temperature 196 °C385 °FExtrusion
 193 - 232 °C380 - 450 °FProcessing
Mold Temperature 10.0 - 51.7 °C50.0 - 125 °FProcessing
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Moisture Content 0.080 %0.080 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiProcessing
 5.00 - 20.0 MPa725 - 2900 psiExtrusion
Clamp Pressure 41.4 - 68.9 MPa6000 - 10000 psi
Vent Depth 0.00254 cm0.00100 in
Cushion 0.317 - 0.635 cm0.125 - 0.250 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Change in Mass in IRM 903 Oil at 257°F for 70 hr97
ColorBlack
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PADVA080 / 22770

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.