MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Llumar Mirage V38 SR CDF Window Film
Categories: Polymer; Film

Material Notes: Dual-Reflective films offer superior energy savings through lower interior reflectivity and higher exterior reflectivity allowing for excellent views to the outside both day and night. Dual-Reflective films are suggested for residential and commercial applications where heat and glare are the primary concerns.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 39 %39 %
UV Transmittance 30 %30 %Solar
Reflection Coefficient, Visible (0-1) 0.170.17Visible Reflectance (interior)
 0.260.26Total Solar Reflectance
 0.260.26Visible Reflectance (exterior)
 
Descriptive Properties
% Glare Reduction57
% Summer Solar Heat Gain Reduction50
% Total Solar Energy Rejected57
% Ultraviolet Ray Protection (wavelengths 300-380nm)>99
% Winter Heat Loss Reduction3
Emissivity0.78
Light to solar gain (LSG)0.91
Shading coefficient0.49
Solar absorption44
Solar Heat Gain Coefficient0.43
U-value1.01Winter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5452 / 222646

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.