MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Abatron Primkote 8006-1 All Purpose Epoxy Primer
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Primkote 8006-1 is an all purpose epoxy primer that excels as a primer for concrete, metal, and wood. It also performs well as a penetrating primer for weathered wood, concrete sealer, conditioner for urethanes, and tie-coat between epoxy surfaces. Features: 2-component (1:1 ratio), solvent-based, flexible, fast-drying, and glossy. Benefits: Can be used on both dry and damp surfaces; Water and weather resistant; Heavy-duty performance; Chemical resistant.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 25 %25 %
Volatile Organic Compounds (VOC) Content 240 g/l240 g/lEPA method #24
Viscosity 7.35 cP7.35 cPASTM-D562
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 6.50 MPa943 psiASTM-D4541
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °FASTM-D2485
 
Processing PropertiesMetricEnglishComments
Processing Temperature 15.6 - 29.4 °C60.0 - 85.0 °FApplication Temperature
Tack-Free Time 10.0 min0.167 hour
Pot Life 4320 - 5760 min4320 - 5760 min(3-4 Days); working life
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Hardening Time (min)120
Impact Resistance68ASTM-D4226

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nanocyl PREGCYL™ NC R2HM-01 Pre-impregnated UD/Fabric Carbon Fibers
Solvay Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Solvay Thornel® T-50 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg

PABC838 / 107822

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.