MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lehvoss LUVOCOM® 3F PEKK 50082 NT PEKK for Additive Manufacturing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; PEKK, Unreinforced

Material Notes: Polyetherketoneketone unreinforced, natural

Main features: Low warpage, isotropic shrinkage characteristics. Highly chemically-resistant parts, non flammable.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccISO 1183-3
Water Absorption <= 0.100 %
@Time 86400 sec
<= 0.100 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0100 - 0.0160 cm/cm0.0100 - 0.0160 in/inDIN 16742
Melt Flow 25.4 g/10 min
@Load 2.16 kg,
Temperature 380 °C
25.4 g/10 min
@Load 4.76 lb,
Temperature 716 °F
pellet
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psi50 mm/min; ISO 527
Elongation at Break 5.00 %5.00 %50 mm/min, Fmax; ISO 527
Tensile Modulus 3.00 GPa435 ksi1 mm/min; ISO 527
Flexural Strength 150 MPa21800 psi10 mm/min; ISO 178
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
Flexural Strain at Break 6.00 %6.00 %10 mm/min, Fmax; ISO 178
Charpy Impact Unnotched NBNB80x10x4mm; ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+12 ohm<= 1.00e+12 ohmRonde 60x4mm; DIN EN 62631-3-2
Insulation Resistance <= 1.00e+12 ohm<= 1.00e+12 ohmstrip electrode R25; DIN EN 62631-3-3
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air  255 °C
@Time 7.20e+7 sec
491 °F
@Time 20000 hour
Continuous; IEC 60216
 300 °C
@Time 720000 sec
572 °F
@Time 200 hour
during lifetime
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 340 - 370 °C644 - 698 °F
Zone 1 320 - 350 °C608 - 662 °F
Zone 2 340 - 370 °C644 - 698 °F
Zone 3 340 - 370 °C644 - 698 °F
Melt Temperature 380 °C716 °F
Drying Temperature  120 °C
@Time 21600 - 36000 sec
248 °F
@Time 6.00 - 10.0 hour
Dehumidifying
 140 °C
@Time 14400 - 21600 sec
284 °F
@Time 4.00 - 6.00 hour
Dehumidifying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8733 / 325117

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.