MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.

Uses: Blown and flat die/cast film extrusion, Injection and blow molding.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provide by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 89 - 95
@Time 5.00 sec
89 - 95
@Time 0.00139 hour
ASTM D2240
Tensile Strength 58.99 MPa8556 psi28 days immersion in Diesel Fuel
 60.85 MPa8826 psi15 days immersion in Diesel Fuel
 62.1 MPa9010 psiASTM D412
Elongation at Break 500 %500 %ASTM D412/D638
100% Modulus 7.60 MPa
@Strain 100 %
1100 psi
@Strain 100 %
ASTM D412
300% Modulus 20.7 MPa
@Strain 300 %
3000 psi
@Strain 300 %
ASTM D412
Tear Strength 26.3 kN/m150 pliTrouser; ASTM D470
Graves Tear Strength 99.9 kN/m570 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 4040H18, 1000g; ASTM D3389
Tensile Set 21 %21 %200% elongation; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 °C284 °FDSC
Vicat Softening Point 83.9 °C183 °FASTM D1525
Glass Transition Temp, Tg -25.0 °C-13.0 °FDSC
 
Processing PropertiesMetricEnglishComments
Zone 1 182 °C360 °FExtrusion
Zone 2 188 °C370 °FExtrusion
Zone 3 193 °C379 °FExtrusion
Zone 4 199 °C390 °FExtrusion
Adapter Temperature 204 °C399 °F5, Extrusion
Die Temperature 204 °C399 °FZone 1, 6, Extrusion
 204 °C399 °FZone 2, Extrusion
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Volume swell in Diesel Fuel8%24 hr, ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Covestro Desmopan® 3690AU Polyurethane
Covestro Desmopan® 3065D Polyurethane
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane

PNOVEON038 / 55304

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.