MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Silver-flo™ 67E Easy Silversmithing Solder
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silver-flo™ 67X, 67E, 67H, Silver-flo™ 74M, and Silver-flo™ 81En are cadmium free silver brazing filler metals designed for use on silver and silver alloys. They are used by silversmiths and referred to as ‘solders’. These filler metals are often simply described by using their traditional names ‘Easy’, ‘Extra Easy’ etc. These names describe the relative melting temperatures of the ‘solders’, ‘Extra Easy’ being the lowest and ‘Hard’ being the highest.

Each ‘solder’ has a minimum 66.7% of silver and hence can be used as a hallmarking grade ‘silver solder’ on sterling silver. Apart from the Silver-flo™ 81En these ‘solders’ generally have good melting ranges and are therefore relatively free flowing. They produce neat joints with small fillets and also provide a good color match with silver alloys. These characteristics make them ideal for joining silver alloys in jewelry or silversmithing applications.

Here a ‘solder’ with a high melting point and with a low zinc content is required so that the enameling process neither re-melts the soldered joints nor causes the zinc in the ‘solder’ to volatilize.

Primarily used for joining sterling / standard silver and other high silver content alloys used in the silversmithing industry.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 705 - 723 °C
Solidus 705 °C
Liquidus 723 °C
 
Descriptive Properties
Size3 x 0.5 x 600mm
Weight (per strip)9g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey Silver-flo™ 81En Enameling Silversmithing Solder
Johnson Matthey Silver-flo™ 74M Medium Silversmithing Solder
Johnson Matthey Silver-flo™ 67H Hard Silversmithing Solder

NJMMJ9774 / 186175

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.