MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALCOM® LDDC PMMA 1000 UV 18124 BK1074-11 PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, UV Stabilized, Molded

Material Notes: Base Polymer: Polymethylmethacrylate

Filler/Additive System: UV stabilized

Special Features: Translucent

Market Segment: Automotive, Lighting

Application Area: Lighting, light transparent components, Black Panel-Technology

Typical Application: Lamp covers, display elements, operating elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Time 86400 sec
0.0060 - 0.0080 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 69.0 MPa10000 psiISO 527
Elongation at Break 4.0 %4.0 %ISO 527
Tensile Modulus 3.30 GPa479 ksiISO 527
Flexural Strength 100 MPa14500 psiISO 178
 96.0 MPa
@Strain 3.5 %
13900 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 3.30 GPa479 ksiISO 178
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -40.0 °C
9.52 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 2.10 J/cm²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C192 °FISO 75-1/-2
Vicat Softening Point 107 °C225 °FB50; ISO 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Glow Wire Flammability Index  650 °C
@Thickness 1.00 mm
1200 °F
@Thickness 0.0394 in
passed; DIN EN 60695
 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
passed; DIN EN 60695
 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
passed; DIN EN 60695
 650 °C
@Thickness 4.00 mm
1200 °F
@Thickness 0.157 in
passed; DIN EN 60695
 
Optical PropertiesMetricEnglishComments
Haze  3.0 %
@Thickness 1.00 mm
3.0 %
@Thickness 0.0394 in
A,2°; ISO 13468
 4.5 %
@Thickness 4.00 mm
4.5 %
@Thickness 0.157 in
A,2°; ISO 13468
Transmission, Visible  4.5 %
@Thickness 4.00 mm
4.5 %
@Thickness 0.157 in
A,2°; ISO 13468
 41.5 %
@Thickness 1.00 mm
41.5 %
@Thickness 0.0394 in
A,2°; ISO 13468
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 280 °C410 - 536 °FInjection molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °FInjection molding
Drying Temperature  65.0 - 90.0 °C
@Time 14400 - 21600 sec
149 - 194 °F
@Time 4.00 - 6.00 hour
in an circulating dryer
 65.0 - 90.0 °C
@Time 10800 - 14400 sec
149 - 194 °F
@Time 3.00 - 4.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolymethylmethacrylate
Half Power Angled=1mm, A,2°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
European Oak Wood
Arkema Altuglas® 84 L Acrylic-Styrene Copolymer
Plaskolite West Optix® CA-41 General Purpose Acrylic Resin
Overview of materials for Acrylic, Glass Fiber Reinforced

PALBIS8481 / 242540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.