MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Information provided by Allvac and the references. Annealed 705ºC. Alpha-Beta Alloy.

Characteristics: High strength at elevated temperatures, heat-treatable, good hardenability, weldable.

Applications: Intermediate-temperature jet engine applications. Blades, discs, spacers, seals.

Forms typically available: Billet, bar, plate and sheet.

4 other heat treatments of this alloy are listed in MatWeb.

Key Words: Ti-6246; Titanium 6-2-4-6; UNS R56260
Vendors:
TITANIUM ENGINEERS is your source for high strength, NACE titanium alloys, with a full range of stock sizes and sizes made to order. Our in-house metallurgical experts ensure the best alloy selection and process titanium to meet unique customer specifications. Please visit our website www.TitaniumEngineers.com for more information or call us at +1 281 265 2910 (USA) or +44 (0) 1675 464200 (UK).

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 342Estimated from Rockwell C.
Hardness, Knoop 373Estimated from Rockwell C.
Hardness, Rockwell C 37
Hardness, Vickers 358Estimated from Rockwell C.
Tensile Strength, Ultimate 1110 MPa
Tensile Strength, Yield 1020 MPa
Elongation at Break 15 %
Tensile Modulus 114 GPa
Poissons Ratio 0.33Typical for alpha-beta titanium alloy.
Fatigue Strength 290 MPa
@# of Cycles 1.00e+7
notched
 620 MPa
@# of Cycles 1.00e+7
Unnotched
Fracture Toughness 26.0 MPa-m½K(IC)
Shear Modulus 42.9 GPaCalculated from typical values.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000190 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.60 µm/m-°C
@Temperature 20.0 °C
 9.90 µm/m-°C
@Temperature 205 °C
 10.4 µm/m-°C
@Temperature 540 °C
Specific Heat Capacity 0.500 J/g-°C
Thermal Conductivity 7.70 W/m-K
@Temperature 23.0 °C
 13.5 W/m-K
@Temperature 540 °C
Melting Point 1595 - 1675 °C
Solidus 1595 °C
Liquidus 1675 °C
Beta Transus 935 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 6.0 %
Carbon, C <= 0.040 %
Iron, Fe <= 0.15 %
Molybdenum, Mo 6.0 %
Nitrogen, N <= 0.040 %
Oxygen, O <= 0.12 %
Tin, Sn 2.0 %
Titanium, Ti 82 %
Zirconium, Zr 4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STA-1
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) BSTA
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STOA
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STA-2
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age

MTP625 / 14238

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.