MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company ESD 300 EM FR Polycarbonate (PC), ESD Protection - Static Dissipative - Flame Retardant - Easy Molding - UL94  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9300 psiASTM D 638
Elongation at Break 8.0 - 12 %ASTM D 638
Tensile Modulus 400 ksiASTM D 638
Flexural Strength 15500 psiASTM D 790
Flexural Modulus 400 ksiASTM D 790
Izod Impact, Notched 0.800 ft-lb/in
@Thickness 3.17 mm
D 256
Izod Impact, Unnotched 28.0 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 10000 ohm-cmASTM D 257
Surface Resistivity per Square <= 1.00e+7 ohmASTM D 257
Static Decay <= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 550 - 600 °F
Mold Temperature 180 - 250 °F
Drying Temperature 250 °F
Dry Time 4 hour
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company ESD 300 EM TFE 15 Polycarbonate (PC), ESD Protection - Static Dissipative - Easy Molding - PTFE Lubricated
Techmer ES Electrafil® PC-50/EC/VO Polycarbonate, Conductive Carbon Filled
Röhm Plexiglas® 8N PMMA Molding Compound
Trinseo Plexiglas® V825-UVA5A Acrylic
RTP Company RTP 383 FR Polycarbonate (PC), Carbon Fiber - Flame Retardant - UL94 V-0

PQZWA1437 / 90810

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.