MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 1503-40D TFE 20 SI 2  Polyester Elastomer (TPE) Glass Fiber 20% - PTFE 20% - Silicone 2% - 40 Shore D  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP; Polyester Thermoplastic Elastomer, Glass Filled

Material Notes: Glass Fiber 20% - PTFE 20% - Silicone 2% - 40 Shore D

Comments:

  • Glass Fiber
  • PTFE Lubricated
  • Silicone Lubricated
  • 40-D Durometer

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Filler Content 20 %
Linear Mold Shrinkage 0.0020 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40ASTM D2240
Tensile Strength, Ultimate 3000 psiASTM D412
Modulus of Elasticity 150 ksiASTM D412
Flexural Yield Strength 3200 psiASTM D790
Flexural Modulus 120 ksiASTM D790
Izod Impact, Notched 9.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 10.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 120 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
Per testing by RTP Company; ASTM D635
 
Processing PropertiesOriginal ValueComments
Processing Temperature 380 - 450 °F
Mold Temperature 70.0 - 120 °F
Injection Pressure 10000 - 15000 psi
 
Descriptive Properties
ColorNatural

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CPT C-Flex® R70-085 Clear Biocompatible TPE
CPT C-Flex® R70-190 Opaque Biocompatible TPE
RTP Company RTP 1500-40D TFE 15 SI  Polyester Elastomer (TPE) PTFE 15% - Silicone - 40 Shore D
Precision Polymer Engineering S80U Silicone Rubber
Master Bond EP21SC-1 Two Component Epoxy Resin System

PR4834 / 64161

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.