MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chesterton MRS S2 Metal Rebuilding System
Categories: Ceramic

Material Notes: An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is formulate for the resurfacing of metal components subjected to extreme corrosive to severe fluid flow conditions. MRS S2 is a low viscosity composite that is designed to be spray applied but may also be applied by roller or brush. This product is formulated as a two coat system to provide extended wear life for plant equipment. Cured MRS S2 provides a high gloss ceramic surface with resistance to erosion-corrosion.

Benefits:

  • High gloss finish reduces drag, improves pump efficiency on worn components
  • Tough resin structure resists thermal-mechanical shock
  • Outstanding adhesion insures reliable performance against under film corrosion.
  • Labor and downtime are reduced due to ease of application and rapid curing
  • Convenient 2-1 volumetric mix ratio and verification of mix by color change
  • Performs well under fluctuating chemical environments

Suggested Uses:

  • Fans & Housings
  • Heat Exchangers
  • Hoppers
  • Tank Linings
  • Valve Assemblies
  • Waterboxes
  • Cooling Water Systems
  • Pump Components
  • Scrubber Systems
  • Pipeline Coatings

    Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D2240
Tensile Strength at Break 6700 psiASTM D638
Elongation at Break 4.0 %ASTM D638
Flexural Strength 11000 psiASTM D790
Flexural Modulus 790000 psiASTM D790
Compressive Strength 9400 psiASTM D695
Adhesive Bond Strength 2100 psiLap Shear; ASTM D1002
Taber Abrasion, mg/1000 Cycles 31
@Load 1.00 kg
H-18 (loss); ASTM D4060
Abrasion 2.4[%]Weight Loss; Federal Test Method Spec. 6193 Modified
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °CWet
 175 °CDry
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 hour
@Temperature 32.0 °C
Light Load
 10.0 hour
@Temperature 25.0 °C
Light Load
 10.0 hour
@Temperature 32.0 °C
Overcoat End
 14.0 hour
@Temperature 32.0 °C
Full Load
 18.0 hour
@Temperature 16.0 °C
Light Load
 20.0 hour
@Temperature 25.0 °C
Overcoat End
 24.0 hour
@Temperature 10.0 °C
Light Load
 24.0 hour
@Temperature 25.0 °C
Full Load
 24.0 hour
@Temperature 32.0 °C
Full Chemical
 30.0 hour
@Temperature 16.0 °C
Overcoat End
 40.0 hour
@Temperature 10.0 °C
Overcoat End
 48.0 hour
@Temperature 16.0 °C
Full Load
 48.0 hour
@Temperature 25.0 °C
Full Chemical
 60.0 hour
@Temperature 10.0 °C
Full Load
 96.0 hour
@Temperature 16.0 °C
Full Chemical
 120 hour
@Temperature 10.0 °C
Full Chemical
Tack-Free Time 1.00 hour
@Temperature 32.0 °C
 2.00 hour
@Temperature 25.0 °C
 3.00 hour
@Temperature 16.0 °C
 6.00 hour
@Temperature 10.0 °C
 
Descriptive Properties
ColorGray
 Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Master Builders Solutions ChemRex® CX-943 Squeegee-grade Polyurethane Adhesive
BASF Master Builders Solutions ChemRex® CX-941 Polyurethane Adhesive
Anderman Ceramics EC100P Recrystallized Silicon Carbide
Aluminum Nitride, AlN
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material

PPTCHS124 / 138236

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.