MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 84 Organic Acid, Water Soluble Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Excellent for Copper and difficult-to-solder metals including Alloy 42, Alloy 51, and Nickel alloys
  • Effective on bare Copper, OSP, HASL, or plated surfaces
  • May be applied in either foam or spray systems
  • Solders single- and double-sided circuit boards
  • Conforms to IPC ANSI J-STD-004, Type ORM1.
Description: Superior No. 84 is a high activity halide, organic acid (OA) foam flux formulated for difficult-to-solder surfaces where activated rosin fluxes and less active OA fluxes cannot be used. This flux combines a unique activation system with a special no-polyol base that is compatible with all solder masks, does not leave a post-solder white residue, and is an ideal choice for high volume soldering operations. The solderability and cleanability of Superior No. 84, along with excellent foaming characteristics and heat stability, provide a moderately low “solids” flux adaptable to a wide variety of board styles, sizes and thicknesses.

Applications: WAVE SOLDERING-To ensure optimum flux activity, a topside temperature of 88-116°C/190-240°F is recommended. Residues from Superior No. 84 are completely water-soluble and can be removed in batch or in-line aqueous cleaning systems. For best cleaning results, wash residues immediately after soldering. A water temperature of 49-60°C/120-140°F is recommended for optimum results. However, excellent results are routinely achieved at lower water temperatures. The organic base of Superior No. 84 is non-toxic and low foaming. Rinse waters are completely biodegradable. Consult local authorities for disposal regulations.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.825 - 0.871 g/cc
Density 6.95 lb/gal
Solids Content 17 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 190 - 240 °CTopside Temperature
Flash Point 53.0 °CTCC Method
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 315 °CSoldering Range
Shelf Life 2.00 Month
 
Descriptive Properties
FormClear liquid, pale yellow
Halide Content3.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX034 / 185718

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.