MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black color.

Benefits: The product offers an excellent combination between thermal and mechanical properties as well as a low warpage of molded parts.

Available in: Asia Pacific, Europe, Latin America and North America.

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: This grade is commonly used in the automotive industry to mould large parts such as rocker cover and engine covers.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183/A
Water Absorption 1.0 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Viscosity 30 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
 30 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
 30 cP
@Shear Rate 1000 1/s,
Temperature 300 °C
 105 cP
@Shear Rate 100 1/s,
Temperature 300 °C
 109 cP
@Shear Rate 100 1/s,
Temperature 290 °C
 120 cP
@Shear Rate 100 1/s,
Temperature 280 °C
Linear Mold Shrinkage 0.0065 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0066 cm/cm
Linear Mold Shrinkage, Transverse 0.0101 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaISO 527 Type 1A
 150 MPaASTM D638
Tensile Stress at Strain 22.0 MPa
@Strain 1 %,
Temperature 120 °C
 30.0 MPa
@Strain 1 %,
Temperature 80.0 °C
 45.0 MPa
@Strain 2 %,
Temperature 120 °C
 50.0 MPa
@Strain 1 %,
Temperature 23.0 °C
 60.0 MPa
@Strain 2 %,
Temperature 80.0 °C
 60.0 MPa
@Strain 5.0 %,
Temperature 120 °C
 61.0 MPa
@Strain 8.0 %,
Temperature 120 °C
 78.0 MPa
@Strain 5.0 %,
Temperature 80.0 °C
 80.0 MPa
@Strain 8.0 %,
Temperature 80.0 °C
 130 MPa
@Strain 2 %,
Temperature 23.0 °C
Elongation at Break 2.0 %ISO 527 Type 1A
 2.0 %ASTM D638
Tensile Modulus 10000 MPaISO 527 Type 1A
Flexural Strength 210 MPaISO 178
 220 MPaASTM D790
Flexural Modulus 9000 MPaISO 178
 9600 MPaASTM D790
Izod Impact, Notched (ISO) 4.00 kJ/m²ISO 180/1A
Charpy Impact Unnotched 45.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75/Af
 240 °CASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
1210
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 275 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Draw-plate temperatures280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled
Akro-Plastic Akromid® B3 (2500) PA 6 Dry
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6

PRHOD618 / 137849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.