MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lushan PR298 Polypropylene Copolymer Adhesive for Steel Pipe Coating
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Polypropylene copolymer adhesive resin Lushan PR298 is maleic grafted polymer in granule form. It is a high tech product and was developed by Guangzhou Hot-melt Adhesive Engineering and Technical R&D Center. Polypropylene copolymer adhesive resin Lushan PR298 is used as adhesive layer between epoxy powder layer and PP compound top coats layer. Polypropylene copolymer adhesive resin Lushan PR298 been exported to many countries all over the world, and successfully applied to wrapped coated or direct coated 3PP buried anti-corrosion steel pipe and coated steel plastic composite pipe for exploration and transportation of natural gas, oil, chemical liquids, water, etc.

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.892 g/ccASTM D792
Melt Index of Compound 2.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 500 %ASTM D638
Peel Strength >= 100 kN/m90+5°C; ISO 21809-1
 >= 150 kN/m50+5°C; ISO 21809-1
 >= 200 kN/m20+5°C; ISO 21809-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °CASTM D2117
Maximum Service Temperature, Air 110 °C
Vicat Softening Point 130 °CASTM D1525
Minimum Service Temperature, Air -20.0 °C
Brittleness Temperature -30.0 °CASTM D746
 
Descriptive Properties
Appearancegranule

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lushan PR320 Adhesive Resin for Aluminum Plastic Composite Pipe
Lushan M-10A Adhesive Resin for Multi-layer Sausage Casing film
Borealis Borcoat™ BB125E Polypropylene Adhesive for Steel Pipe Coating

PLUSH006 / 150004

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.