MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SCG Chemicals P607F Homopolymer resin
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: SCG PP P607F is homopolymer resin without slip and antiblock agent, and suitable for cast film application as a core layer of co-extrusion film or monolayer film requiring high film stiffness and high clarity.

Applications: Monolayer cast film, core layer for co-extrusion cast film, metalized film.

Features: Good film stiffness. Good optical property. Low gels. Excellent process ability.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D 1505
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 28.4 MPa4120 psiASTM D882
Film Tensile Strength at Yield, TD 22.6 MPa3280 psiASTM D882
Film Elongation at Break, MD 470 %470 %ASTM D882
Film Elongation at Break, TD 20 %20 %ASTM D882
Flexural Modulus 1.608 GPa
@Thickness 3.00 mm
233.2 ksi
@Thickness 0.118 in
ASTM D790
2% Secant Modulus 0.382 GPa55.4 ksiTD; ASTM D882
 0.510 GPa74.0 ksiMD; ASTM D882
Film Tensile Strength at Break, MD 36.3 MPa5260 psiASTM D882
Film Tensile Strength at Break, TD 8.82 MPa1280 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 162 °C324 °FASTM D2117
Vicat Softening Point 154 °C309 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 1.3 %1.3 %ASTM D1003
Gloss 84 %84 %ASTM D2457
 
Descriptive Properties
AppearancePellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC781 / 278038

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.