MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ PVDF 2066_0002 Fluoroplastic
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: 3M™ Dyneon™ PVDF 2066/0002, a fluoropolymer material, provides an excellent balance of physical properties, processability, surface smoothness, flexibility, and refractive index, allowing for a wide array of gauges for filaments such as fishing line. In addition to the well established intrinsic characteristics of PVDF such as high strength for a given filament diameter and a refractive index nearly identical to water, PVDF 2066/0002 has improved impact resistance that can provide additional shock strength to filament
    Features and Benefits:
  • Highest impact strength of any extrudable 3M PVDF
  • Highest melt viscosity of any extrudable 3M PVDF
  • High tensile strength

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 4.0 - 6.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 67.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 46.0 MPa50 mm/min; ASTM D638
Elongation at Break 428 %50 mm/min; ASTM D638
Elongation at Yield 9.0 %50 mm/min; ASTM D638
Flexural Modulus 1670 MPa50 mm/min; ASTM D790
 
Descriptive Properties
ColorOpaque
Volatile Matter<0.2%5 min/110°, Thermobalance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade 7B Granular Compression Molding Resin
Overview of materials for Silicone Rubber
Silicon, Si
Ti30Nb ß titanium alloy
AGC Fluon® FEP 100 White Pigmentation

PDYL9975 / 129993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.