Data provided by the manufacturer, Exxon Chemical. A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film. Applications: Packing films (cling). Data for film properties below based on 1.25 mil film. |
Ethylene Vinyl Acetate; Exxon Chemical Company |