(Viewing data as-entered.
Click here
to return)
LG Chemical LGflex EBNW Plasticizer
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
Material Notes:
Features: Excellent Adhesion, Transparency, and Non-endocrine disrupter
Application: PVC Food Package Wrap
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
0.991
-
0.997
g/cc
Volatiles
8.0 %
@Time 3600 sec
Loss
17.2 %
@Time 7200 sec
Loss
Viscosity
18
cP
Molecular Weight
383
g/mol
Chemical Properties
Original Value
Comments
Acid Value
<= 0.20
KOH mg/g
<= 0.50
After Heating, KOH mg/g
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
21.6
MPa
Elongation at Break
445 %
50% Modulus
0.00451
GPa
@Strain 50 %
100% Modulus
0.00706
GPa
@Strain 100 %
Thermal Properties
Original Value
Comments
Melting Point
-21.0
°C
Freezing Point
Boiling Point
337
°C
Flash Point
220
°C
Descriptive Properties
Color
<100 APHA
Flexible Temperature
-15 kg/cm
2
G=3.17x10
3
Heat Loss
<1%
125°Cx3hr, JIS K6751
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
LG Chemical LGflex GL300 Plasticizer
LG Chemical LGflex GL100 Plasticizer
LG Chemical LGflex BET Plasticizer
LG Chemical DOP Plasticizer
LG Chemical DOA Plasticizer
PLAY252 / 148262
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.