Styrene-Butadiene Copolymer Description: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 602 provides good fluidity properties to the compound while keeping good mechanical properties. Applications: Thanks to it very high crumb porosity Finaprene® 602 is designed for the compounding industry. This crumb shape, along with the broad molecular weight distribution confer a quick oil absorption to the polymer and lead to the production of fluid compounds. This fluidity will enhance the surface aspect of the injected article. The structure of 602 is n = 2, 3, 4, 5. Content of the compound for which the listed properties apply: F484: 0 F435: 83 F411x: 17 F602: 0 F507: 12.5 GPPS: 32 HIPS: 0 Oil: 56 CaCO3: 10 Additional Notes: DIN Abrasion: 155 mm³ Data provided by Total Petrochemicals. Total Petrochemicals includes former Fina and Atofina plastics product lines. |