MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

PolyPLASTY PolyJARID PA 6 G Polyamide 6 cast, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes:
  • Polyamide casted: Semi-products and parts weighing up to 2 tons
  • Machined parts: Turned and milled parts in single and serial production

Information provided by PolyPLASTY.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 2.8 %2.8 %under regular conditions; ISO 62
Moisture Absorption at Equilibrium 8.0 %8.0 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, H358/30 160 MPa23200 psiISO 2039-1
Tensile Strength, Yield 90.0 MPa13100 psiISO 527
Elongation at Break 20 %20 %ISO 527
Modulus of Elasticity 3.60 GPa522 ksiISO 527
Flexural Strength 140 MPa20300 psiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1C
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1C
Tensile Creep Modulus, 1000 hours 2300 MPa334000 psi0.5 percent; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 100 kV/mm
@Thickness 0.600 mm
2540 kV/in
@Thickness 0.0236 in
IEC 60243-1
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359
Specific Heat Capacity 1.68 J/g-°C0.402 BTU/lb-°FIEC 1006
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FDIN 52 612
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 80.0 °C176 °Flong term
 150 °C302 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FISO 75
Vicat Softening Point 215 °C
@Load 5.10 kg
419 °F
@Load 11.2 lb
point B; ISO 306 VST/B/50
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
IEC 60695-11-10
 
Descriptive Properties
LOI Acid Index (%)25ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for ECTFE Fluoropolymer
Covestro Desmopan® 790 Polyurethane
3D Systems QuickPlastic Cast Urethane Material GlassFilled Nylon

PPOLYPL923 / 197633

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.